| Measurement method |
Hot Wire Method |
| Range |
0.023 - 12 W/m • K (standard probe) |
| Precision |
±5%/reading of reference plate |
| Reproducibility |
±3%/reading of reference plate |
| Temperature |
-10 - 200°C Note: thermal bath is necessary for other
than room temperature |
| Measuring time |
60 seconds Note: sample piece must be thermally in
equilibrium. |